The spontaneous broken rate of clear tempered  glass is less than 0.1% after HST. Because low iron glass has the characteristics of low iron content and high purity, the spontaneous broken rate of tempered low iron glass products that have undergone HST is even lower.

Our low iron tempered glass products after HST, have no spontaneous broken (breakage) so far.

15mm, 878*6000mm tempered low iron glass produced for Malaysian customers is undergoing HST.